Speed
m/min20
Energy saving
%2
Temperature control
℃The precision rolling tube induction type bright solid solution production line has significant characteristics such as small footprint, low energy consumption, no need for preheating, and can also work online with the rolling mill to meet the requirements of ultra long tube bright heat treatment process. The performance of the pipe meets the national standard GBT4334-2008 (300 series and 2205 dual phase steel) for intergranular corrosion.
CONSULTWith bright annealing, pipe cleaning, and pipe polishing.
Traceable temperature, solution power, and current frequency of each steel pipe.
Ensure that the quality of the welded pipe meets ASME standards, with a speed of up to 1~8m/min
The yield can reach over 98%.
Connecting the upstream rolling mill to achieve ultra long pipes.
With one click start stop function.
Material | 304L/N/LN, 316L, 317L, and other 300 series stainless steel, 2205 dual phase steel, and nickel based alloys. |
---|---|
Outer diameter | Φ6~25mm |
Wall thickness | 0.5~2.0mm |
Heat-treatment temperature | 1050~1150℃ |
Speed | 1~5m/min |
Temperature Accuracy | ±2℃ |
Pipe length | 30~101m |